Concrete creep testing machine is designed to determine concrete cylinder and cuboid parts under a constant pressure for a set period. It is also suitable for concrete creep deformation test under single-direction pressure at constant temperature in a humid-free environment.
| Capacity | 500kN/1000kN |
| Measurement range | 0-500kN/0-1000kN |
| Relative reading error | ±1% |
| Spring height | 300mm |
| Spring compression stroke | 52mm (or customized) |
| Max. distance between upper platen and lower platen (Compression space) | 1500mm (or customized) |
| Power supply | 220V, 50Hz |
| Overall dimension (without packing) | 750×750×2800mm |
| Net weight | About 800kg |
Note: all platens are produced by CNC machine with surface treatment. All platens and columns are made of No. 45 steel.